欧美性猛交黑人软件,丰满人妻熟妇丰满av无码,亚洲中国日韩午夜精品无码,女生挤奶啪啪网站不卡

        當前位置:首頁(yè)-新聞資訊

        檢查鋁板生產(chǎn)廠(chǎng)家質(zhì)量如何該檢查哪些?

        來(lái)源:http://www.gytimber.com/ 發(fā)布時(shí)間:2018-05-14

        1.標識的檢查
        1. identification check
        平常我們看到的花紋鋁板廠(chǎng)家都是具有標識的,而且標識上是有產(chǎn)品的標準代號和許可證的。
        Usually we see the pattern of aluminum plate manufacturers are marked, and the logo is the product's standard code and license.
        2.表面質(zhì)量的檢查
        2. inspection of surface quality
        在花紋鋁板廠(chǎng)家的表面除了要看清潔與否之外,我們需要看到更多的東西,比如我們應該看看鋁板材是否出現了一些裂痕或者出現了一些腐蝕的現象,這些都是需要仔細的觀(guān)察的才能發(fā)現的。
        In addition to the surface of the planed aluminum manufacturer, we need to see more, for example, we should see if there are some cracks in the aluminum sheet or some corrosion phenomena that need to be carefully observed.
        3.氧化膜的厚度
        Thickness of 3. oxide film
        這個(gè)是需要使用的渦流測厚儀器進(jìn)行檢測。
        This is a professional eddy current thickness gauge.

        鋁卷生產(chǎn)廠(chǎng)家
        4.封孔的質(zhì)量
        The quality of 4. holes
        封孔的形成是在進(jìn)行的陽(yáng)極氧化后才形成的,如果這些封孔沒(méi)有很好的處理的話(huà),就會(huì )導致以后的鋁板材被腐蝕的現象出現。通常我們進(jìn)行的檢測方法是酸浸法,就是除去表面額灰塵之后,將硝酸滴到表面,進(jìn)行輕輕的擦拭之后,用水洗掉硝酸,再在表面滴上紫藥水,一分鐘后搽干凈,看看表面是否有明顯的痕跡,如果有的話(huà)就說(shuō)明封孔沒(méi)有處理的很好。
        The formation of the sealing hole is formed after the anodization of the anode. If these sealing holes are not treated well, it will lead to the corrosion of the later aluminum sheet. We usually test the method of acid leaching, that is, after removing the surface dust, drop the nitric acid on the surface, then wash the nitric acid with water and drop the purple water on the surface. After a minute, we can see if there is any obvious trace on the surface, if the fruit has some words, it shows that the sealing hole is not treated. Very good.
        5.耐蝕性
        5. corrosion resistance
        花紋鋁板廠(chǎng)家這個(gè)指標也是影響到鋁板材的壽命的,我們經(jīng)常使用的是滴堿的方法,使用的是氫氧化鈉溶液,主要是看氧化膜被貫穿的時(shí)間。建議在實(shí)驗室里有嚴格要求的情況下進(jìn)行。。
        This indicator is also affecting the life of aluminum plate, we often use the method of drop alkali, the use of sodium hydroxide solution, mainly to see the time of the oxide film through. It is suggested that there should be strict requirements in the laboratory.

        有了上面的小總結,希望對廣大客戶(hù)有所幫助,如果有什么不理解的或者尋求幫助的請點(diǎn)擊我們的官方網(wǎng)站:鋁卷生產(chǎn)廠(chǎng)家http://www.gytimber.com或者來(lái)電咨詢(xún),我們會(huì )盡全力為您解決
        With a small summary above, I hope to be helpful to our customers. If there is anything that is not understood or if you are looking for help, please click on our official website: the aluminum producer http://www.gytimber.com or the call consultation, we will do our best to solve the problem.