        油污會(huì )對鋁卷的外觀(guān)造成很大的危害

        來(lái)源:http://www.gytimber.com/ 發(fā)布時(shí)間:2022-12-29

        油污是指鋁卷軋制后鋁尖表面油過(guò)多.除軋制油膜外,還含有多余的油,肉眼可見(jiàn)于分切生產(chǎn)和產(chǎn)品檢驗,這些油主要是由輥頸或軋機出口上下甩、濺、滴在箱面、軋機清輥器異常、軋機測厚頭滴油等形成的,往往臟成分凌亂。
        Oil stain refers to excessive oil on the surface of aluminum tip after aluminum coil rolling. In addition to rolling oil film, it also contains excess oil, which can be seen visually in slitting production and product inspection. The oil is mainly formed by roll neck or mill outlet throwing up and down, splashing, dropping on the box surface, abnormal mill cleaner, and oil dripping from the thickness measuring head of the mill, and the dirty ingredients are often messy.
        鋁卷生產(chǎn)廠(chǎng)家提醒您,這種油污會(huì )對鋁卷的外觀(guān)造成很大的危害:一是鋁卷產(chǎn)品大多作為裝飾或包裝材料,須有干凈的外觀(guān);二是厚度薄,后續退火容易形成氣泡,影響使用,由于油量大,這里殘留過(guò)多。油污的缺點(diǎn)是評價(jià)鋁箔質(zhì)量的一個(gè)非常重要的指標。
        The aluminum coil manufacturer reminds you that this oil stain will cause great harm to the appearance of aluminum coil. First, aluminum coil products are mostly used as decoration or packaging materials, and must have a clean appearance; Second, the thickness is thin, and subsequent annealing is easy to form bubbles, affecting the use. Due to the large amount of oil, there is too much residue here. The defect of oil stain is a very important index to evaluate the quality of aluminum foil.

        鋁卷生產(chǎn)廠(chǎng)家
        在生產(chǎn)過(guò)程中嚴格檢查生產(chǎn)設備。如發(fā)現設備內油污過(guò)多,應及時(shí)清洗,找出原因,同時(shí)對生產(chǎn)產(chǎn)品進(jìn)行板面清洗加工。不能清洗的產(chǎn)品無(wú)效的,禁止油污產(chǎn)品入庫流入商場(chǎng)。
        Strictly check the production equipment during production. If too much oil stain is found in the equipment, it shall be cleaned in time to find out the cause, and the production products shall be cleaned and processed at the same time. If the products that cannot be cleaned are invalid, oil contaminated products are prohibited from entering the store.
        此外劃痕、劃痕、劃痕是鋁卷表面的間歇性或連續的單溝傷痕。一般來(lái)說(shuō),當尖銳物與箔表面接觸后相對滑動(dòng)時(shí)。軋輥、導輥表面有尖缺點(diǎn),或粘有硬雜物;機械導輥、剪切、卷、分切機械導輥、導線(xiàn)有尖缺點(diǎn)或枯萎雜物。劃痕:束(或組)分布的疤痕由于物體之間的邊緣和表面,或表面與表面接觸后相對滑動(dòng)或錯誤。
        In addition, scratches, scratches are intermittent or continuous single groove scars on the aluminum coil surface. Generally speaking, when the sharp object slides relative to the foil surface after contact. The surface of roll and guide roll has sharp defects or is stuck with hard debris; Mechanical guide roller, shear, roll, slitting mechanical guide roller and wire have sharp defects or withered impurities. Scratches: The scars distributed by bundles (or groups) are relatively sliding or wrong due to the edges and surfaces between objects, or after the surface contacts with the surface.
        之所以說(shuō)油污會(huì )對鋁卷的外觀(guān)造成很大的危害的原因便是以上內容了,您可以作為使用參考信息看,更多相關(guān)事項就來(lái)我們網(wǎng)站http://www.gytimber.com咨詢(xún)!
        The reason why the oil stain will cause great harm to the appearance of the aluminum coil is that the above contents can be used as reference information, and more relevant matters can be found on our website http://www.gytimber.com consulting service